Base Fe (Iron) : Fe52-62 / Ni28-32 / Si5-6 / Cr4.5-5.5 / Mn0.5-1.5 Impurities: C<2.6, Cu<0.5, P<0.08 Tradename: NI-RESIST TYPE 4 Elements Symbol Elements Name Min Max % C (carbon) 0 2.6 % Cr (chromium) 4.5 5.5 % Cu (copper) 0 0.5 % Fe (iron) 51.8 62 % Mn (manganese) 0.5 1.5 % Ni (nickel) 28 32 … Continue reading EN GJSA XNiSiCr30 5 5 Cast Iron Chemical Composition (austenitic, nodular) | Modulus Metal | Supplier Company | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY