Base Fe (Iron) : Fe56-64 / Ni34-36 / Si1.5-3 / Mn0.5-1.5 Impurities: C<2.4, Cu<0.5, Cr<0.2, P<0.08 Elements Symbol Elements Name Min Max % C (carbon) 0 2.4 % Cr (chromium) 0 0.2 % Cu (copper) 0 0.5 % Fe (iron) 56.3 64 % Mn (manganese) 0.5 1.5 % Ni (nickel) 34 36 % P (phosphorus) … Continue reading EN GJSA XNi35 Cast Iron Chemical Composition (austenitic, nodular) | Modulus Metal | Supplier Company | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY