Base Fe (Iron) : Fe66-76 / Ni21-24 / Mn1.5-2.5 / Si1-3 Impurities: C<3, Cr<0.5, Cu<0.5, P<0.08 Elements Min Max % C (carbon) 0 3 % Cr (chromium) 0 0.5 % Cu (copper) 0 0.5 % Fe (iron) 66.4 76.5 % Mn (manganese) 1.5 2.5 % Ni (nickel) 21 24 % P (phosphorus) 0 0.08 % … Continue reading EN GJSA XNi22 Cast Iron Chemical Composition (austenitic, nodular) | Modulus Metal | Supplier Company | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY