INCOLOY 800 Material Data Sheet (Cold drawn, Bar)
Nickel-Fe-Cr alloy, INCOLOY 800, cold drawn, bar INCOLOY 800 Designation (cold drawn, bar) Unified Numbering System (USA): N08800 Condition Cold drawn UNS number N08800 US name ASTM Grade N08800; AMS 5766, 5871 EN name X 10 NiCrAlTi 32 20 EN number 1.4876 ISO name ISO 9723, 9724, 9725, 6207, 6208 INCOLOY 800 Tradenames (cold drawn, … Continue reading INCOLOY 800 Material Data Sheet (Cold drawn, Bar)