Hy-Tuf Low Alloy Steel Mechanical Properties
Hy-Tuf Low Alloy Steel Mechanical Properties Hy-Tuf Condition Quenched & tempered Young’s modulus 200 – 210 GPa Specific stiffness 25.5 – 26.9 MN.m/kg Yield strength (elastic limit) 1280 – 1410 MPa Tensile strength 1520 – 1680 MPa Specific strength 163 – 180 kN.m/kg Elongation 5 – 10 % strain Compressive strength 1330 – 1470 MPa … Continue reading Hy-Tuf Low Alloy Steel Mechanical Properties