EN GJN HV600 (XCr23) Equivalent Grades, former BS 3E, Cast iron, white, high-chromium alloy
UNS number F45009 EN GJN HV600 (XCr23), former BS 3E, Cast iron, white, high-chromium alloy Equivalent Grades Designation BS EN 12513:2011 EN GJN HV600 (XCr23) (former BS 3E). Record based on BS 4844:1986 BS grade 3E. Standards with similar compositions: GB 8491(87) KmTBCr26 (China) AFNOR NFA32401 FBCr26MoNi (France) DIN G-X260Cr27 (Germany) DIN G-X300CrMo271 (Germany) DIN … Continue reading EN GJN HV600 (XCr23) Equivalent Grades, former BS 3E, Cast iron, white, high-chromium alloy