EN GJN HV600 (XCr14) Chemical Composition, former BS 3A, Cast iron, white, high-chromium alloy

Compositional summary Fe69-84 / Cr14-18 / C1.8-3.6 / Mn0.15-1.5 (impurities: Mo<3, Cu<2, Ni<2, Si<1, P<0.1, S<0.1) Material family: Metal (ferrous) Base material: Fe (Iron) Elements Min Max % C (carbon) 1.8 3.6 % Cr (chromium) 14 18 % Cu (copper) 0 2 % Fe (iron) 68.8 84.1 % Mn (manganese) 0.15 1.5 % Mo (molybdenum) … Continue reading EN GJN HV600 (XCr14) Chemical Composition, former BS 3A, Cast iron, white, high-chromium alloy