EN GJN HV350 Equivalent Grades, former BS 1C, Cast iron, white, low alloy

Designation BS EN 12513:2011 EN GJN HV350 (former BS 1C). Record based on BS 4844:1986 BS grade 1C. Tradenames: CY/A, CY/H, MEEHANITE WEC Standards with similar compositions: France:                  FBA to AFNOR NF A32-401, FBO to AFNOR NF A32-401 India:                     Grade 1 to IS 7925, Grade 3 to IS 7925 UK:                        1A to BS 4844, 1C … Continue reading EN GJN HV350 Equivalent Grades, former BS 1C, Cast iron, white, low alloy