EN 1561 Standard Guide Founding — Grey cast irons Overview KEY POINTS What is Grey Cast Iron? Cast iron with carbon present mainly as flake (lamellar) graphite Application Sand moulds or moulds with comparable thermal behaviour Main Grades 5 grades by tensile strength + 6 grades by hardness Key Feature Properties depend on wall thickness … Continue reading EN 1561 Standard Guide