LDX2101 Duplex Stainless Steel Material Data Sheet
Stainless steel, duplex, LDX2101, annealed LDX2101 Duplex Stainless Steel Designation Wrought S-Steel:Duplex LDX 2101 Condition Solution annealed UNS number S32101 EN number 1.4162 LDX2101 Duplex Stainless Steel Composition detail C (carbon) 0 – 0.04 % Cr (chromium) 21 – 22 % Cu (copper) 0.1 – 0.8 % Fe (iron) 67.3 – 73.2 % Mn (manganese) … Continue reading LDX2101 Duplex Stainless Steel Material Data Sheet