ASTM CD-4MCu, cast, water quenched, Duplex Stainless Steel Material Data Sheet
Stainless steel, duplex, ASTM CD-4MCu, cast, water quenched ASTM CD-4MCu Designation ASTM CD-4MCu Condition Solution annealed; water quenched UNS number J93370 US name ASTM CD-4MCu ASTM CD-4MCu Typical uses Chemicals industry, marine, water supply, power plant, pulp & paper manufacture, soap manufacture, textiles, transportation ASTM CD-4MCu Composition detail C (carbon) 0 – 0.04 % Cr … Continue reading ASTM CD-4MCu, cast, water quenched, Duplex Stainless Steel Material Data Sheet