AISI 329 Duplex Stainless Steel Material Data Sheet 

Stainless steel, duplex, AISI 329, annealed AISI 329 Duplex Stainless Steel Designation AISI 329, wrought Condition Annealed UNS number S32900 US name SAE 329, ASTM S32900, ~ASTM S32950, ~ASTM F52 EN name X8CrNiMo27-5 EN number ~1.4460 ISO name X3CrNiMoN27-5-2 GB (Chinese) name 0Cr26Ni5Mo2 JIS (Japanese) name SUS329J1TP, ~SUS329J4L, ~SUS329J3L AISI 329 Duplex Stainless Steel Typical … Continue reading AISI 329 Duplex Stainless Steel Material Data Sheet