AISI 2205 Duplex Stainless Steel Material Data Sheet

Stainless steel, duplex, AISI 2205, annealed AISI 2205, annealed, Duplex Stainless Steel Designation Wrought S-Steel: AISI 2205, annealed Condition Solution annealed UNS number S31803 – S32205 US name ASTM S32205, ASTM S31803, ASTM F60, ASTM F51 EN name X2CrNiMoN22-5-3 EN number 1.4462 ISO name X2CrNiMoN22-5-3 JIS (Japanese) name SUS329J3L AISI 2205, annealed, Duplex Stainless Steel … Continue reading AISI 2205 Duplex Stainless Steel Material Data Sheet