Aluminum 5251 Material Data Sheet

Aluminum 5251 (annealed) Material Data Sheet Aluminum 5251 Designation 5251, wrought Condition O (Annealed) UNS number A95251 EN name EN AW-5251 (EN AW-Al Mg2) EN number 3.3525 Aluminum 5251 Typical uses Sheet metal work, marine applications – seawater desalination equipment, cryogenic use, welded pressure vessels, commercial vehicle trim, shipbuilding applications – hulls & superstructures, can … Continue reading Aluminum 5251 Material Data Sheet