Aluminum 5182 Material Data Sheet

Aluminum 5182 (annealed) Material Data Sheet Aluminum 5182 Designation 5182, wrought Condition O (Annealed) UNS number A95182 EN name EN AW-5182 ISO name Al Mg4,5Mn0,4 Aluminum 5182 Typical uses Automotive body sheet, reinforcement members, brackets and parts. Uses in metal sheet, packaging, can stock and container ends. Aluminum 5182 Composition detail Al (aluminum) 93.2 – … Continue reading Aluminum 5182 Material Data Sheet