Aluminum 5086 Material Data Sheet

Aluminum 5086 (annealed) Material Data Sheet Aluminum 5086 Designation 5086, wrought Condition O (Annealed) UNS number A95086 EN name EN AW-5086 (EN AW-Al Mg4) EN number 3.3545 Aluminum 5086 Typical uses Marine, automotive, and aircraft parts, cryogenics, TV towers, drilling rigs, transportation equipment, missile components, armor plate. Applications requiring weldable moderate-strength alloy having comparatively good … Continue reading Aluminum 5086 Material Data Sheet