Aluminum 5083 Material Data Sheet

Aluminum 5083 (annealed) Material Data Sheet Aluminum 5083 Designation 5083, wrought Condition O (Annealed) UNS number A95083 EN name EN AW-5083 (EN AW-Al Mg4,5Mn0,7) EN number 3.3547 TAluminum 5083 ypical uses Marine, auto, and aircraft applications, unfired welded pressure vessels, cryogenics, TV towers, drilling rigs, transportation equipment, missile components, armor plate. Applications requiring a weldable … Continue reading Aluminum 5083 Material Data Sheet