Aluminum 5052 Material Data Sheet

Aluminum 5052 (annealed) Material Data Sheet Aluminum 5052 Designation 5052, wrought Condition O (Annealed) UNS number A95052 EN name EN AW-5052 (EN AW-Al Mg2,5) EN number 3.3523 Aluminum 5052 Typical uses Aircraft fuel and oil lines, fuel tanks, miscellaneous marine and transport applications, sheet metal work, appliances, street light standards, rivets, and wire. Applications where … Continue reading Aluminum 5052 Material Data Sheet