Aluminum 5005 Material Data Sheet

Aluminum 5005 (annealed) Material Data Sheet Aluminum 5005 Designation 5005, wrought Condition O (Annealed) UNS number A95005 EN name EN AW-5005 (EN AW-Al Mg1(B)) EN number 3.3315 Aluminum 5005 Typical uses Appliances, cooking utensils, architectural applications, commercial vehicle trim, shipbuilding applications – hulls & superstructures, can manufacture & cooking utensils, truck bodies, road tankers, vehicle … Continue reading Aluminum 5005 Material Data Sheet