Aluminum 356.0 vs A356.0 (Permanent mold cast, T6)

Aluminum 356.0 vs A356.0 (Permanent mold cast, T6) The differences between Aluminum 356.0 and Aluminum A356.0, both in the permanent mold cast, T6 condition: Property Aluminum 356.0 Aluminum A356.0 Designation 356.0 (Aluminum Association) A356.0 (Aluminum Association) UNS Number A03560 A13560 EN Number EN AC-42000 / EN AC-Al Si7Mg EN AC-42000 / EN AC-Al Si7Mg Typical … Continue reading Aluminum 356.0 vs A356.0 (Permanent mold cast, T6)