Aluminum, 333.0, Permanent Mold Cast, T6 | Mechanical Properties

Mechanical Properties for Aluminum 333.0 Property Value Range Unit Young’s Modulus 72.5 – 75.5 GPa Specific Stiffness 26.1 – 27.3 MN·m/kg Yield Strength (Elastic Limit) 197 – 217 MPa Tensile Strength 290 – 319 MPa Specific Strength 71 – 78.6 kN·m/kg Elongation 1.5 – 1.8 % strain Compressive Strength 197 – 217 MPa Flexural Modulus … Continue reading Aluminum, 333.0, Permanent Mold Cast, T6 | Mechanical Properties