Mechanical Properties for Aluminum 333.0

PropertyValue RangeUnit
Young’s Modulus72.5 – 75.5GPa
Specific Stiffness26.1 – 27.3MN·m/kg
Yield Strength (Elastic Limit)197 – 217MPa
Tensile Strength290 – 319MPa
Specific Strength71 – 78.6kN·m/kg
Elongation1.5 – 1.8% strain
Compressive Strength197 – 217MPa
Flexural Modulus72.5 – 75.5GPa
Flexural Strength (Modulus of Rupture)207 – 228MPa
Shear Modulus27.1 – 28.6GPa
Bulk Modulus67.9 – 77.7GPa
Poisson’s Ratio0.322 – 0.338
Shape Factor31
Hardness (Vickers)111 – 123HV
Elastic Stored Energy (Springs)262 – 319kJ/m³
Fatigue Strength at 10⁷ Cycles92.7 – 113MPa
Fatigue Strength Model (Stress Range)89.6 – 117MPa
Aluminum, 333.0, Permanent Mold Cast, T6 | Mechanical PropertiesUNS Number A03330 Mechanical Properties

MODULUS METAL | ALUMINUM CASTING FOUNDRY IN TURKEY
Aluminium Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Plaster Casting in Turkey, Heat Treated and CNC Machined Products Manufacturer in Turkey