Standards with Similar Compositions for Aluminum 333.0

RegionStandard
USA333, 333 to ASTM B108, 333 to QQ A-596, 333.1, 333.1 to ASTM B179, 333.1 to QQ A-371F

A03330 to SAE J452, A333.0, A333.1, D380.0, D380.1, UNS A03330, UNS A03331, UNS A13330, UNS A13331

UNS A43800, UNS A43801