Aluminum, 333.0, Permanent Mold Cast, T6 | Composition
Composition Overview for Aluminum 333.0 Category Details Compositional Summary Al 82-89 / Si 8-10 / Cu 3-4 / Mg 0.05-0.5 (Impurities: Fe <1, Zn <1, Mn <0.5, Ni <0.5, Ti <0.25, Other <0.5) Material Family Metal (non-ferrous) Base Material Al (Aluminum) Aluminum, 333.0, Permanent Mold Cast, T6 Composition Overview UNS Number A03330 Composition Overview Detailed … Continue reading Aluminum, 333.0, Permanent Mold Cast, T6 | Composition