Composition Overview for Aluminum 333.0

CategoryDetails
Compositional SummaryAl 82-89 / Si 8-10 / Cu 3-4 / Mg 0.05-0.5 (Impurities: Fe <1, Zn <1, Mn <0.5, Ni <0.5, Ti <0.25, Other <0.5)
Material FamilyMetal (non-ferrous)
Base MaterialAl (Aluminum)
Aluminum, 333.0, Permanent Mold Cast, T6 Composition Overview UNS Number A03330 Composition Overview

Detailed Composition

ElementRange (%)
Al (Aluminum)81.8 – 89
Cu (Copper)3 – 4
Fe (Iron)0 – 1
Mg (Magnesium)0.05 – 0.5
Mn (Manganese)0 – 0.5
Ni (Nickel)0 – 0.5
Si (Silicon)8 – 10
Ti (Titanium)0 – 0.25
Zn (Zinc)0 – 1
Other0 – 0.5
Aluminum, 333.0, Permanent Mold Cast, T6 Detailed CompositionUNS Number A03330 Detailed Composition