AISI 304LN Stainless Steel Material Data Sheet

AISI 304LN Stainless Steel Material Data Sheet Stainless steel, austenitic, AISI 304LN, annealed AISI 304LN General information Designation AISI 304LN, wrought Condition Solution annealed UNS number S30453 US name ASTM WP304LN, ASTM TP304LN, ASTM TP304L, ASTM S30454, ASTM S30453, ASTM S30403, ASTM F304NL, ASTM F304LN, ASTM CR304LN, ASTM 304LN, ASTM 18Cr8Ni modified with N, ASME … Continue reading AISI 304LN Stainless Steel Material Data Sheet