AISI 301 Stainless Steel Material Data Sheet

AISI 301 Stainless Steel Material Data Sheet Stainless steel, austenitic, AISI 301, annealed AISI 301 Stainless Steel General information Designation AISI 301, wrought Condition                          Solution annealed UNS number S30100 US name ASTM S30100, ASTM MT-301, ASME 301, ~AMS 5519, ~AMS 5518, ~AMS 5517 EN name ~X5CrNi17-7, ~X2CrNiN18-7, ~X10CrNi18-8 EN number ~1.4319, ~1.4318, ~1.4310 ISO name … Continue reading AISI 301 Stainless Steel Material Data Sheet