AISI 216 Stainless Steel Mechanical Properties
AISI 216 Stainless Steel Mechanical Properties (Annealed) Young’s modulus 190 – 201 GPa Specific stiffness 24.3 – 25.8 MN.m/kg Yield strength (elastic limit) 345 – 450 MPa Tensile strength 620 – 760 MPa Specific strength 44.2 – 57.7 kN.m/kg Elongation 37 – 43 % strain Compressive strength 345 – 450 MPa Flexural modulus 190 – … Continue reading AISI 216 Stainless Steel Mechanical Properties
Copy and paste this URL into your WordPress site to embed
Copy and paste this code into your site to embed