AISI 216 Stainless Steel Chemical Composition

AISI 216 Stainless Steel Composition C (carbon) 0 – 0.08 % Cr (chromium) 17.5 – 22 % Fe (iron) 57.6 – 67.8 % Mn (manganese) 7.5 – 9 % Mo (molybdenum) 2 – 3 % N (nitrogen) 0.25 – 0.5 % Ni (nickel) 5 – 7 % P (phosphorus) 0 – 0.045 % S (sulfur) … Continue reading AISI 216 Stainless Steel Chemical Composition