ADI 900 Austempered Ductile Cast Iron Thermal Properties
ADI 900 Thermal Properties Melting point 1110 – 1190 °C Maximum service temperature 350 – 450 °C Minimum service temperature 0 °C Thermal conductivity 21.2 – 22.8 W/m.°C Specific heat capacity 460 – 495 J/kg.°C Thermal expansion coefficient 12.5 – 16.5 µstrain/°C Thermal shock resistance 213 – 294 °C Thermal distortion resistance 1.33 … Continue reading ADI 900 Austempered Ductile Cast Iron Thermal Properties