ADI 900 Austempered Ductile Cast Iron Mechanical Properties

ADI 900 Mechanical Properties Young’s modulus 163 – 170 GPa Specific stiffness 23 – 24 MN.m/kg Yield strength (elastic limit) 550 – 650 MPa Tensile strength 900 – 995 MPa Specific strength 77.6 – 91.7 kN.m/kg Elongation 8 – 11 % strain Compressive modulus 163 – 170 GPa Compressive strength 1280 – 1490 MPa Flexural … Continue reading ADI 900 Austempered Ductile Cast Iron Mechanical Properties