ADI 800 Austempered Ductile Cast Iron Mechanical Properties

ADI 800 Mechanical properties Young’s modulus 163 – 170 GPa Specific stiffness 22.9 – 24 MN.m/kg Yield strength (elastic limit) 454 – 530 MPa Tensile strength 750 – 837 MPa Specific strength 63.9 – 74.7 kN.m/kg Elongation 10 – 12 % strain Compressive modulus 163 – 170 GPa Compressive strength 1250 – 1480 MPa Flexural … Continue reading ADI 800 Austempered Ductile Cast Iron Mechanical Properties