ADI 1600 Austempered Ductile Cast Iron Mechanical Properties
ADI 1600 Mechanical properties Young’s modulus 155 – 163 GPa Specific stiffness 21.9 – 23.1 MN.m/kg Yield strength (elastic limit) 1260 – 1470 MPa Tensile strength 1600 – 1770 MPa Specific strength 178 – 208 kN.m/kg Elongation 1 – 2 % strain Compressive modulus 155 – 163 GPa Compressive strength 2340 – 2710 MPa Flexural … Continue reading ADI 1600 Austempered Ductile Cast Iron Mechanical Properties