ADI 1400 Austempered Ductile Cast Iron Mechanical Properties
ADI 1400 Mechanical properties Young’s modulus 156 – 165 GPa Specific stiffness 22 – 23.4 MN.m/kg Yield strength (elastic limit) 1030 – 1240 MPa Tensile strength 1400 – 1550 MPa Specific strength 146 – 175 kN.m/kg Elongation 1 – 3 % strain Compressive modulus 156 – 165 GPa Compressive strength 2030 – 2350 MPa Flexural … Continue reading ADI 1400 Austempered Ductile Cast Iron Mechanical Properties