ADI 1050 Austempered Ductile Cast Iron Mechanical Properties

ADI 1050 Mechanical properties Young’s modulus 160 – 168 GPa Specific stiffness 22.6 – 23.7 MN.m/kg Yield strength (elastic limit) 730 – 866 MPa Tensile strength 1050 – 1200 MPa Specific strength 103 – 122 kN.m/kg Elongation 6 – 10 % strain Compressive modulus 160 – 168 GPa Compressive strength 1530 – 1790 MPa Flexural … Continue reading ADI 1050 Austempered Ductile Cast Iron Mechanical Properties