ISO 1461 vs ISO 2081 vs ISO 19598
ISO 1461 vs ISO 2081 vs ISO 19598 Table 1: Scope and Process Overview Feature ISO 1461 ISO 2081 ISO 19598 Primary Process Hot Dip Galvanizing: Dipping fabricated articles into molten zinc. Electroplating: Electrodeposition of zinc. Electroplating: Electrodeposition of zinc or zinc alloys. Substrate Fabricated iron and steel articles (including castings). Iron or steel. Iron … Continue reading ISO 1461 vs ISO 2081 vs ISO 19598