ISO 1461 Hot dip galvanized coatings on fabricated iron and steel articles -Specifications and test methods. 1. Scope & Application Category Description ✅ Applies To Batch Hot Dip Galvanizing of fabricated iron and steel articles (including certain castings). ❌ Excludes Continuous sheet, wire, and woven/welded mesh. ❌ Excludes Tube and pipe galvanized in automatic plants. … Continue reading ISO 1461 Hot dip galvanized coatings on fabricated iron and steel articles -Specifications and test methods