EN 13858 Corrosion protection of metals — Non-electrolytically applied zinc flake coatings on iron or steel components Designations General The designation shall consist of the following:a) term “non-electrolytically applied”;b) number of this European Standard, EN 13858;c) hyphen (-);d) chemical symbol of the basis metal;e) stroke (/);f) symbols for the zinc flake coating and the method … Continue reading EN 13858 Zinc Flake Coatings