AISI 202 Stainless steel (Low nickel general purpose), austenitic | 1/4 hard | Mechanical Properties  

Modulus Metal | Manufacturer Company in TURKEY: Sand Casting | Investment Casting | Foundry | CNC Machining | Press Bending | Laser Cutting | Welding | Plastics Injection Molding | Turkiye Mechanical properties Values Young’s modulus * 190 – 210 GPa Specific stiffness * 24.3 – 27 MN.m/kg Yield strength (elastic limit) 515 – 670 MPa … Continue reading AISI 202 Stainless steel (Low nickel general purpose), austenitic | 1/4 hard | Mechanical Properties