AISI 201 Stainless steel (Low nickel work hardenable), austenitic | Carbon equivalency
Carbon equivalency: 0.775 – 1.13 Modulus Metal | Manufacturer Company in TURKEY: Sand Casting | Investment Casting | Foundry | CNC Machining | Press Bending | Laser Cutting | Welding | Plastics Injection Molding | Turkiye