Modulus Metal | Manufacturer Company in TURKEY: Sand Casting | Investment Casting | CNC Machining | Press Bending | Laser Cutting | Welding | Plastics Injection Molding Composition detail % C (carbon)  0 – 0.15 % Cr (chromium)  16 – 18 % Fe (iron) * 67.5 – 75 % Mn (manganese)  5.5 – 7.5 % … Continue reading AISI 201 Stainless steel (Low nickel work hardenable), austenitic | Chemical Composition