AISI 201 Stainless steel (Low nickel work hardenable), austenitic, Annealed | Mechanical Properties

Modulus Metal | Manufacturer Company in TURKEY: Sand Casting | Investment Casting | CNC Machining | Press Bending | Laser Cutting | Welding | Plastics Injection Molding Mechanical properties Values Young’s modulus  193 – 201 GPa Specific stiffness  24.7 – 25.9 MN.m/kg Yield strength (elastic limit)  275 – 350 MPa Tensile strength  655 – 950 … Continue reading AISI 201 Stainless steel (Low nickel work hardenable), austenitic, Annealed | Mechanical Properties