EN GJS 600 3 Cast iron, nodular graphite, Mechanical Properties Young’s modulus 170 – 180 GPa Flexural modulus * 170 – 180 GPa Shear modulus 66 – 71 GPa Bulk modulus 123 – 137 GPa Poisson’s ratio 0.27 – 0.28 Shape factor 22 Yield strength (elastic limit) 370 – 415 MPa Tensile strength 600 – … Continue reading EN GJS 600 3 Cast iron, nodular graphite, Mechanical Properties | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY