EN GJS 500 7 Cast iron, nodular graphite, Mechanical Properties Young’s modulus 165 – 178 GPa Flexural modulus * 165 – 178 GPa Shear modulus 64 – 71 GPa Bulk modulus 119 – 135 GPa Poisson’s ratio 0.27 – 0.28 Shape factor 23 Yield strength (elastic limit) 320 – 370 MPa Tensile strength 500 – … Continue reading EN GJS 500 7 Cast iron, nodular graphite, Mechanical Properties | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY