EN GJS 600 3 Chemical Composition (Cast iron, nodular graphite) | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY

Base Fe (Iron) : Fe/3.3-3.8C/2-3Si/<1.0Ni/0.2-0.5Mn/0.02-0.07Mg Material Standards with Similar Chemical Composition NBN 830-02 FNG50-7 (Belgium) GB 1348(88) QT 500-7 (China) DS 11303 727 (Denmark) AFNOR NFA32201 FGS500-7 (France) DIN WNr 0.7050 (Germany) DIN 1693 GGG-50 (Germany) IS 1865 SG500/7 (India) UNI 4544 GS500-7 (Italy) JIS G5502(95) FCD50 Class 3 (Japan) NEN 2733 GN500-7 (Netherlands) NS … Continue reading EN GJS 600 3 Chemical Composition (Cast iron, nodular graphite) | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY