EN GJS 400 18U Chemical Composition (Cast iron, nodular graphite) | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY

Base Fe (Iron) : Fe/3.4-4C/2-2.8Si/0.2-0.6Mn/0.02-0.07Mg Material Standards with Similar Chemical Composition NBN 830-02 FNG38-17 (Belgium) GB 1348(88) QT 400-15 (China) GB 1348(88) QT 400-18 (China) DS 11303 715 (Denmark) DS 11303 716 (Denmark) AFNOR NFA32201 FGS350-22 (France) AFNOR NFA32201 FGS350-22L (France) AFNOR NFA32201 FGS400-15 (France) AFNOR NFA32201 FGS400-18 (France) AFNOR NFA32201 FGS400-18L (France) DIN WNr … Continue reading EN GJS 400 18U Chemical Composition (Cast iron, nodular graphite) | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY