Base Fe (Iron) : Fe/3.2-4.1C/1.8-2.8Si/<0.8Mn/<0.1P/<0.03S Material Standards with Similar Chemical Composition NBN 830-02 FNG38-17 (Belgium) GB 1348(88) QT 400-15 (China) GB 1348(88) QT 400-18 (China) DS 11303 715 (Denmark) DS 11303 716 (Denmark) AFNOR NFA32201 FGS350-22 (France) AFNOR NFA32201 FGS350-22L (France) AFNOR NFA32201 FGS400-15 (France) AFNOR NFA32201 FGS400-18 (France) AFNOR NFA32201 FGS400-18L (France) DIN WNr … Continue reading EN GJS 400 18 Chemical Composition (Cast iron, nodular graphite) | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY