NBN 830-02 FNG50-7 (Belgium)GB 1348(88) QT 500-7 (China)DS 11303 727 (Denmark)AFNOR NFA32201 FGS500-7 (France)DIN WNr 0.7050 (Germany)DIN 1693 GGG-50 (Germany)IS 1865 SG500/7 (India)UNI 4544 GS500-7 (Italy)JIS G5502(95) FCD50 Class 3 (Japan)NEN 2733 GN500-7 (Netherlands)NS 11301 NS11350 (Norway)AS 1831(85) 500-7 (NSW Australia)GOST 7293 VCh50 (Russian Federation)SABS 936 SG50 (South Africa)SIS 140727 0727-02 (Sweden)ISO 1083(87) 500-7 (International)BS … Continue reading Cast iron, nodular graphite, EN GJS 600 3 Equivalent Grades | Modulus Metal | Supplier | Foundry | Castings Products | in TURKEY